nanoindentation相关论文
在利用电迁移现象制备铝纳米线的过程中, 铝纳米线的生长位置取决于铝原子的积聚位置。为实现铝原子积聚位置控制, 基于纳米压痕技......
利用离子辅助电子束双源共蒸发工艺方法, 制备了SiO2掺杂含量分别为0、13%、20%、30%、40%和100%的六组HfO2-SiO2混合膜。采用纳米......
Microstructural homogeneity and mechanical behavior of a selective laser melted Ti-35Nb alloy produc
Although using elemental powder mixtures may provide broad alloy selection at low cost for selective laser melting(SLM),......
Thermomechanical cyclic quenching and tempering (TMCT) can strengthen steels through a grain size reduction mechanism. T......
In coal mining industry,with the depth growing of coal mines,the creep behaviours of coal and rock can extensively affec......
Mechanical characterization of Pinus massoniana cell walls infected by blue-stain fungi using in sit
Characterizing the mechanical properties of wood cell walls will lead to better understanding and optimization of modifi......
该文从挂篮荷载计算、施工流程、支座及临时固结施工、挂篮安装及试验、合拢段施工、模板制作安装、钢筋安装、混凝土的浇筑及养生......
The controllable wire bonding of individual Ag nanowires onto a Au electrode was achieved at room temperature. The plast......
ZrO2/Ni nanocomposite was produced via pulse electrodeposition using a nickel sulfmate bath. The effects of main factors......
Mechanical and Wear Properties of Nanostructured Surface Layer in Iron Induced by Surface Mechanical
该文从挂篮荷载计算、施工流程、支座及临时固结施工、挂篮安装及试验、合拢段施工、模板制作安装、钢筋安装、混凝土的浇筑及养生......
Investigation on Aging-induced Softening of Eutectic Microstructure in SnBi/Cu Interconnect by Nanoi
该文从挂篮荷载计算、施工流程、支座及临时固结施工、挂篮安装及试验、合拢段施工、模板制作安装、钢筋安装、混凝土的浇筑及养生......
该文从挂篮荷载计算、施工流程、支座及临时固结施工、挂篮安装及试验、合拢段施工、模板制作安装、钢筋安装、混凝土的浇筑及养生......
Combination of Instrumented Nanoindentation and Scanning Probe Microscopy for Adequate Mechanical Su
The elastic indentation modulus and hardness of standard bulk materials and advanced thin films were deter-mined by usin......
该文从挂篮荷载计算、施工流程、支座及临时固结施工、挂篮安装及试验、合拢段施工、模板制作安装、钢筋安装、混凝土的浇筑及养生......
Effect of heat treatment on the microstructure and micromechanical properties of the rapidly solidif
该文从挂篮荷载计算、施工流程、支座及临时固结施工、挂篮安装及试验、合拢段施工、模板制作安装、钢筋安装、混凝土的浇筑及养生......
该文从挂篮荷载计算、施工流程、支座及临时固结施工、挂篮安装及试验、合拢段施工、模板制作安装、钢筋安装、混凝土的浇筑及养生......
该文从挂篮荷载计算、施工流程、支座及临时固结施工、挂篮安装及试验、合拢段施工、模板制作安装、钢筋安装、混凝土的浇筑及养生......
Mechanical characterization and strain-rate sensitivity measurement of Ti-7333 alloy based on nanoin
The relationship between crystal orientations and meso-mechanical properties of βphase Ti-7333 titanium was investigate......
Determination of elastic and plastic mechanical properties of dentin based on experimental and numer
为探究吕家坨井田地质构造格局,根据钻孔勘探资料,采用分形理论和趋势面分析方法,研究了井田7......
This paper reviews some of the nanoindentation research that has been done on teeth and discusses the usefulness of this......
Molecular dynamics simulations of nanoindentation are performed on monocrystal copper. A new 'contact atoms' met......
Nanoindentation measurement was performed to evaluate the local hardness distribution for quenched and tempered martensi......
Six kinds of micro bridge-beam specimens with different sizes are fabricated using photolithography technology for bendi......
The mechanical behaviour of trabecular bone is dependent on both the properties of individual trabeculae as well as thei......
In this paper,the nanoindentation simulation on the two models of neat polyethylene (PE) and the polyethylene incorporat......
Mechanical and Wear Properties of Nanostructured Surface Layer in Iron Induced by Surface Mechanical
A porosity-free and contamination-free surface layer with grain sizes ranging from nanometer to micrometer in Fe samples......
The multilayer gradient CrN/ZrN coatings were synthesized by a dual cathode DC magnetron sputtering.The influence of dif......
Microbridge testing was used to measure the Youngs modulus and residual stress of metallic films. Samples of freestandin......
Nanoindentation tests were conducted to investigate the near-surface mechanical properties of the individual components ......
A film growth mechanism, expressed in terms of depositing hard films onto the soft substrate, was proposed. Multicompone......
Indentation creep behaviors of Mg61Cu28Gd11 and (Mg61Cu28Gd11)99.5Sb0.5 bulk metallic glasses at roo
The room temperature creep behaviors of Mg61Cu28Gd11 and (Mg61Cu28Gd11i)99.5Sb0.5 bulk metallic glasses (BMGs) were reve......
通过纳米压痕蠕变实验研究了加载速率对{[(Fe0.6Co0.4)0.75B0.2Si0.05]0.96Nb0.04}96Cr4块体金属玻璃室温蠕变变形的影响。结果表......
通过化学气相沉积方法合成截面为六边形的单晶钨纳米晶须,利用纳米压痕仪和原子力显微镜对硅基底上的钨纳米晶须的力学性能进行表征......
Factors impacting nanoindentation testing results of the cuticle of dung beetle Copris ochus Motschu
The cuticle of dung beetle is a layered composite material in micro- or nano-scale. Dung beetle can fly, walk and dig. I......
The nanoscratch behaviors of La0.7Sr0.3MnO3+δ films, which were deposited with ratio of O2/(O2+Ar), ranging from 4.4% t......
The morphology, composition, and phase structure of the oxide coatings produced on the surface of pure titaniumby altern......
A new type of nano test system was introduced, the test principle and the indentation data analysis method were describe......
Investigation on Aging-induced Softening of Eutectic Microstructure in SnBi/Cu Interconnect by Nanoi
Nanoindentation was used to probe softening of the eutectic microstructure in a SnBi/Cu interconnect following thermal a......
The surface modified nanocopper particles were prepared with chemical reduction method. The wear test was carried out on......
This paper reviews some of the nanoindentation research that has been done on teeth and discusses the usefulness of this......
为探究吕家坨井田地质构造格局,根据钻孔勘探资料,采用分形理论和趋势面分析方法,研究了井田7......
Nanocrystalline hydroxyapatite (HA) powders have been synthesized by precipitation using Ca(NO3)2.4H2O and (NH4)2 HPO4 a......
The deformation behavior and the effect of the loading rate on the plastic deformation in Ce-based bulk metallic glasses......
Plastic deformation behaviors of Zr65Al10Ni10Cu15 and Zr52.5Al10Ni10Cu15Be12.5 bulk metallic glasses (BMGs) are studied ......
Nanoindentation is an attractive characterization technique,as it not only measures the local properties of a material b......
The thin film hardness estimation by nanoindentation is influenced by substrate beyond a critical relative indentation d......
Determination of elastic and plastic mechanical properties of dentin based on experimental and numer
The aim of this study is to investigate the change of mechanical properties of human dentin due to aging and spatial var......